This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
i dont see an image?
what type of Inland PLA, silk generally requires higher temps but some of the more standard ones print well at 180-190.
charmed_electron@programming.dev 10 months ago
Does that top surface feel ridged? To me this looks more like an issue with either overextrusion or z offset too low than temperature.
Nomad@infosec.pub 10 months ago
I second z offset. Weird that this happens only at a certain regular “column”. Could be hiding an underextruded strand on the level below. In that case your temp might not be stable.