Try decreasing the speed in corners and increase pressure advance a bit. There is a tuning print you can use.
Comment on How to properly get rid of holes between perimeters?
Natanox@discuss.tchncs.de 3 weeks agoIt’s not only on the first layer and also not only around corners (indeed the first layer is perfectly fine). The perspective is a little bit misleading, this is the third or fourth layer. Happens on all layers, it’s just a little bit more common around corners and bends.
Nomad@infosec.pub 3 weeks ago
Natanox@discuss.tchncs.de 3 weeks ago
It’s not just in corners.
MrTolkinghoen@lemmy.zip 3 weeks ago
PA can impact more than just corners. It’s when the print head is changing speed/direction
Natanox@discuss.tchncs.de 3 weeks ago
The issue is also present on long straight lines though.
kata1yst@sh.itjust.works 3 weeks ago
Extrusion width?
MrTolkinghoen@lemmy.zip 3 weeks ago
This comment is correct imo. Read / calibrate the pressure advance. I’ve had especially good luck with the adaptive pressure advance and highly recommend taking the time to calibrate it.