I tried a never-used nozzle with no difference.
The bed hasn’t been cleaned in a while, but the parts that aren’t underextruded stick very hard. And it happens the same in every place on the bed (I’ve tried about 8 now, always with the same pattern) and 2 different beds.
I’m still thinking it’s a pressure issue, where it initially doesn’t have enough pressure for some reason. But I turned up the KAMP purge flow and it made no difference, and extruding 2 skirt lines made no difference that I could tell.
My next step is going to give the bed a good cleaning… And even try the other side that I’m pretty sure I’ve never used yet.
wccrawford@lemmy.world 7 months ago
I’ve cleaned the bed and not applied 3DLAC, and it hasn’t helped.
IMALlama@lemmy.world 7 months ago
That’s disappointing. I’m sorry to say, but I’m out of ideas. Maybe try the Voron design forums since they have more active users?