Successful_Try543@feddit.org 2 days agoDeep in the coating, where the Cu6Sn5 [Remark: intermetallic phase of Sn coating and Cu substrate] is present, the deviatoric strain was high. This indicates that the growth of the intermetallic phase causes plastic deformation of the tin coating.
[…]
A short (4 micrometre) radial gradient in hydrostatic stress was observed around the root of the whisker. This gradient together with long-range diffusion from specific regions could provide the driving force for whisker growth.
https://portal.research.lu.se/en/publications/tin-whiskers-experiments-and-modelling