Comment on Newbe advice
HumanPenguin@feddit.uk 3 months agoThanks very useful. More or less what I expected but great to get confirmation. Humidity here is 30 to 60% averaging the higher end more often. So def need decent drying chamber.
Yep, I knew the tent was more about retaining the heat. Just considered the hose a useful add-on. It is good to know you think that will be adequate as I could not find much online.
Do you think mixing colours at diff layers will be an issue as long as I keep both rolls in drying chambers?
Again, thanks for taking the time. It is fantastic to get some confirmations and advice from someone who has used the stuff before I spend what little cash I have.
bigredgiraffe@lemmy.world 3 months ago
Glad to help! Mixing colors shouldn’t be an issue, I have done it in the past, also have mixed PA and PA-CF in the past without issue. I bet you could even find a tent with a window and run a PTFE tube to a dry box outside the tent then you could pull the first color out and put the second one in without having to open the tent.
Also, just to say it out loud I would definitely test the strength of the layer adhesion (especially between the colors since they might have different additives) for anything structural, especially if you might get injured if it fails, just to be double safe heh.
Last, at least where I am, PA is significantly more expensive than ASA or PETG so might be worth looking at those for at least prototypes of the parts. For example, I typically use PLA to prototype ASA parts, has usually been fine to swap it out with just minor tolerance adjustments and it’s way cheaper to print 50 versions in PLA while I’m working out the design and then I print the final ones in ASA or whatever.