Comment on Why prime tower instead of poop?

definitemaybe@lemmy.ca ⁨2⁩ ⁨weeks⁩ ago

I don’t see the full reason anywhere in the thread; the prime tower is essential to quality multicolour prints. Purging quickly shoots out a high volume of filament to quickly clear as much of the previous colour as possible, but then when it goes to start printing, the temperature and pressure are all out of whack and you get inconsistent flow.

So, if you skip the prime tower, you’ll get globby over extrusions and gaps from under extrusion on the first thing printed in that colour each layer, which looks terrible.

That said, the prime tower can be much smaller than default. I set mine to 3mm³ of priming and it comes out 95-100% perfect, with only very occasional blobs on the edge, which pop right off with a fingernail flick (or a deburring tool, if you’re fancy.)

Don’t skip the prime tower. I did for a few weeks before cluing in to why I was getting 1 bad print on every plate.

I suppose if you’re changing filament by layer, then you could maybe skip it, but then definitely don’t print outer wall first or you won’t get a clean print. But even then, a 3mm³ prime tower is tiny, so why risk it?

Hell, even the Snapmaker U1 uses a prime tower, and it has 4 hot ends; it’s needed to normalize the flow after a temperature/flow change (being idle). I don’t have one to test, but I expect it would greatly benefit from a bigger prime tower, since it hasn’t just been extruding filament as purge to get things flowing. But that’s just speculation, as I sadly don’t have one to test with.