Comment on Adhered so hard it delaminated the glass.
IMALlama@lemmy.world 4 weeks agoLifting on the corners, especially if this was a bed sized print, was probably due to warping. It stinks that it took out your bed, but warping probably wasn’t the cause there.
My main printer these days is enclosed. When I print PETG on it I’ll pop the lid open because PETG doesn’t like to be too warm.
hereiamagain@sh.itjust.works 4 weeks ago
I thought too cold caused warping, does too warm cause it as well?
IMALlama@lemmy.world 3 weeks ago
Sorry for the delayed reply. No, too warm won’t cause warping. However, the hold side of your hot end will at best be ambient temperature. If it gets too warm you can clog your nozzle.
My view is “if the chamber doesn’t need to be hotter why make it hotter?”.
If you were printing ASA/ABS you want your chamber to go basically as hot as you can get it though - especially if you’re printing something big.
hereiamagain@sh.itjust.works 3 weeks ago
No worries thanks for the information!