I find that it’s best to use 65C for the bed temperature for the first couple of layers, and then drop the temperature to 50C. If you’re using Cura, there should be an option to do that, but you’ll need to dig through the advanced settings to find it. Doing this has completely solved warping for me (Ender 3 Pro v1 with PLA filament). My understanding is that it works because the temperature differential between the top and bottom layers causes a pulling force that causes the warping that you see. You really only need it to be hot on the initial layer, for the print to stick properly. And afterward you only need to maintain a temp that’s just hot enough that the print doesn’t pop off. Hence, 65C initial, 50C for everything else afterward
Probably less relevant, but I also find that adhesion improves if you have the printer go at half speed for the first couple of layers. Again, there should be a setting in Cura, but it’s in the advanced settings
rambos@lemm.ee 2 months ago
This is correct, shrinking forces are fighting against bed ashesion. I use 60C and then drop it to 55 tho. On top of that you need clean bed and revisit first layer squish