@akilou @over_clox Nono, PLA is also sensitive to humidity. I have seen similar things with filament that I know is dry, so I think it must be something else, and I'm curious what it is.
Overextruding? Have you changed the filament? Sometimes they flow a bit differently.
Comment on Wtf is happening here?
akilou@sh.itjust.works 4 days agoIt’s warming up here and humidity is rising. But it’s never been a problem before and as I understand humidity is more of a PETG thing, this is just PLA
GoblinQuester@dice.camp 4 days ago
FrederikNJS@piefed.zip 4 days ago
While PETG certainly has a lot more moisture problems than PLA, PLA can still give you a lot of grief if it isn’t dry enough. Stringing, oozing, uneven extrusion, and many other weird problems. I would definitely try to dry the filament…
But this could also look a bit like over/under-extrusion… Have you tried calibrating your e-steps?