Comment on delamination on larger surfaces
teotwaki@lemmy.world 1 week agoThe very top layer would also have high cooling fan, no?
It could be your cooling fan is just waaaay too powerful, and causing the plastic to not flow and bond correctly to the lower (or following) layers.
jokeyrhyme@lemmy.ml 1 week ago
According to the print visualisation, there is no cooling at all on the top layer, only on the 3rd-from-the-top layer, which is right above the last sparse infill layer (I have top shell thickness set to 3 layers)